Trelleborg T528 Butyl Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Trelleborg
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg T528 Butyl Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Butyl rubber is a copolymer of isobutylene and a small percentage of isoprene.PropertiesWith careful compounding Butyl has really good tensile strength.Butyl has very low permeability to air and other gases.Excellent resistance to ozone, oxidation and sunlight.Butyl has very low resilience which makes it ideal for vibration damping and shock absorption applications.Butyl has moderate resistance to abrasion and compression set.Resistance to chemicals; resistance to most inorganic products. Highly resistant to mineral acids, alkalines and aqueous acids. Not recommended to use in contact with oils, or hydrocarbon solvents.All information provided by Trelleborg
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Yield 7.00 MPa
1020 psi
Elongation at Break 400 %
400 %
Tear Strength 20.0 kN/m
114 pli
Compression Set 30 %

@Temperature 70.0 °C,
Time 79200 sec
30 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Color Black