UCAR Carbon UCAR® CGW Isostatic Molded Graphite

Category Carbon , Graphite
Manufacturer UCAR Carbon Company (GrafTech International)
Trade Name UCAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UCAR Carbon UCAR® CGW Isostatic Molded Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isostatically molded grade CGW is an ATJ-based material that has been processed to higher density and strength. Grade CGW is characterized by low permeability, erosion resistance and surface hardness.Typical Applications:Continuous casting dies Hot pressing dies and moldsTabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
Particle Size 25 µm
25 µm
Ash 0.090 %
0.090 %
Mechanical Properties Metric English Comments
Flexural Strength 36.5 MPa
5300 psi
Thermal Properties Metric English Comments
CTE, linear 2.90 µm/m-°C

@Temperature 20.0 - 100 °C
1.61 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00117 ohm-cm
0.00117 ohm-cm