Thermal Properties Metric English Comments
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
Ohio Carbon Blank OCB AR-06 EDM Grade Graphite
Available in a range of sizes and shapes.
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
MMCC Cu/Al2O3 Particulate Copper Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
MMCC Cu/B4C Particulate Copper Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
In-Plane; Angstrom's Method
GrafTech eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
In-Plane; Angstrom's Method
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite
Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has..
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® CGW Isostatic Molded Graphite
Isostatically molded grade CGW is an ATJ-based material that has been processed to higher density and strength. Grade CGW is characterized by low permeability, erosion resistance and surface hardnes..
Thermal Conductivity 120 - 150 W/m-K
833 - 1040 BTU-in/hr-ft²-°F
Temper T651
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
Cytec Thornel® P-55S 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the interla..
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
CMW® ELKONITE® TC53 Heat Treatable Tungsten Carbide Copper material
For electroforging and electrical upsetting dies.Information provided by CMW Inc.
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
Ceradyne CeraTrex™ 146-S5 Silicon Carbide
Features:corrosion resistancewear resistancehardnessnet shape fabricationApplications:wear componentsInformation provided by Ceradyne Company