Material Notes:
Construction: ±45° XN50. Fiber: Carbon XN50. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be used in spacecraft Antenna Reflectors, Optical Benches, Solar Arrays, and other lightly loaded structures which must be positioned with accuracy and stability in order to properly perform their intended purpose. It was developed using a space qualified, toughened, polycyanate matrix resin. General Ultracor® features include low density, design flexibility, low CTE, low CME, and high thermal conductivity.Data provided by Ultracor Inc., formerly YLA Cellular Products Company.
Physical Properties Metric English Comments
Density 0.0320 g/cc
0.00116 lb/in³
core density
Mechanical Properties Metric English Comments
Compressive Yield Strength 1.41 MPa
205 psi
Shear Modulus 0.331 GPa
48.0 ksi
ribbon direction
Shear Strength 1.14 MPa
165 psi
ribbon direction
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
across thickness
Thermal Conductivity 1.60 W/m-K
11.1 BTU-in/hr-ft²-°F
transverse to ribbon
2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
ribbon direction
6.00 W/m-K
41.6 BTU-in/hr-ft²-°F
across thickness