Material Notes:
Fiberfrax Durablanket S insulation is a strong, lightweight, flexible needled blanket that is made from spun ceramic fibers. Available in a wide variety of thicknesses, widths and densities, Durablanket S insulation provides an array of proven solutions for a broad spectrum of application problems.Typical ApplicationsFurnace, kiln, reformer and boiler liningsInvestment casting mold wrappingsRemovable insulating blankets for stress relieving weldsReusable insulation for steam and gas turbinesFlexible high-temperature pipe insulationPressure and cryogenic vessel fire protectionHigh-temperature kiln and furnace insulationFurnace door linings and sealsSoaking pit sealsFurnace repairsThermal reactor insulationExpansion joint sealsPrimary reformer header insulationIncineration equipment and stack liningsAnnealing cover sealsHigh-temperature filtrationNuclear insulation applicationsAtmosphere furnace liningField steam generator liningInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Specific Gravity 2.73 g/cc
2.73 g/cc
Density 0.0641 g/cc
0.00231 lb/in³
Available
0.0961 g/cc
0.00347 lb/in³
Available
0.128 g/cc
0.00463 lb/in³
Available
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.0276 MPa
4.00 psi
at 4 PCF; ASTM 686-76
0.0414 MPa
6.00 psi
at 6 PCF; ASTM 686-76
0.0483 MPa
7.00 psi
at 8 PCF; ASTM 686-76
Thermal Properties Metric English Comments
Specific Heat Capacity 1.13 J/g-°C

@Temperature 1093 °C
0.270 BTU/lb-°F

@Temperature 1999 °F
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1177 °C
2151 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 43 - 47 %
43 - 47 %
Alkalis 0.050 %
0.050 %
SiO2 53 - 57 %
53 - 57 %
Descriptive Properties Value Comments
Average Fiber Diameter (microns) 2.5-3.5
Color White
Fiber Diameter (microns) 2.5-3.5
Leachable Chlorides (ppm) <10
Na2O3 (%) <0.5
Other Inorganics (%) 0.85
Temperature Grade (°C) 1260