Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard products offer low thermal conductivity, high temperature stability, uniform density, and excellent resistance to thermal shock and chemical attack.This product possesses the same density and temperature rating as Duraboard RG insulation, but is manufactured to tighter dimensional tolerances and has an excellent finished surface. These characteristics make it ideally suited for use as a sandwich or core material or for use in the manufacture of components where aesthetic quality, as well as uniformity and performance, is important.Description: A higher quality surface finish with tighter dimensional tolerances make this board suitable for use in situations where aesthetic quality, as well as performance, is important.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.256 g/cc
0.00926 lb/in³
Nominal
Loss On Ignition 6.0 - 7.0 %
6.0 - 7.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000552 GPa
0.0800 ksi
Fired (24 hrs at cont. use)
0.00138 GPa
0.200 ksi
Green (typ.)
Compressive Strength 0.152 MPa
22.0 psi
10% Deformation; Fired
0.159 MPa
23.0 psi
5% Deformation; Fired
0.159 MPa
23.0 psi
15% Deformation; Fired
0.290 MPa
42.0 psi
5% Deformation; Green
0.345 MPa
50.0 psi
10% Deformation; Green
0.393 MPa
57.0 psi
15% Deformation; Green
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Shrinkage <= 5.0 %

@Time 86400 sec
<= 5.0 %

@Time 24.0 hour
at Recommended Operating Temperature
Electrical Properties Metric English Comments
Dielectric Strength 1.06 kV/mm
27.0 kV/in
Descriptive Properties Value Comments
Color Cream / white
Fiberfrax® Fibers (%) 100
Temperature Grade (°C) 1260
Copyright © lookpolymers.com All Rights Reserved