Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1150 °C
2100 °F
Dry Air
Outokumpu 353MA® High Temperature Austenitic Stainless Steel
Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but..
Maximum Service Temperature, Air 1150 °C
2100 °F
Dry Air
Outokumpu 4762 High Temperature Ferritic Stainless Steel
Highest chromium content-most resistant to reducing sulphurous gases. Susceptible to 475°C embrittlement and s-phase forms during long exposures in the range 600-800°C.Applications: Mostly used i..
Maximum Service Temperature, Air 1150 °C
2100 °F
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems
Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are f..
Maximum Service Temperature, Air 1149 °C
2100 °F
Pyrotek Pyroboard™ S1150 Roller
Pyroboard™ S1150 is designed for use in an enclosed furnace position where the atmosphere is consistent with strip temperature and does not exceed 2200° F.Information provided by Pyrotek.
Maximum Service Temperature, Air 1150 °C
2100 °F
Gouda Vuurvast CURON 120 HS Dense Refractory Castable
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars...
Maximum Service Temperature, Air 1150 °C
2100 °F
MetalTek MTEK 15-65 Cast UNS N06006 Heat Resistant Stainless Steel
For severe hot gas corrosion resistance at higher temperatures.Applications: Hearth plates, muffles, roller hearths, carburizing boxes.Information provided by MetalTekCast UNS N06006; Cast Grade HX;..
Maximum Service Temperature, Air 1150 °C
2100 °F
for long term exposure
Microtherm Group Super A Alumina Based Thermal Insulation
Microtherm® Super A is an alumina based form of Microtherm® high temperature thermal insulation. It is available in various densities and it is normally supplied without any coating or coverin..
Maximum Service Temperature, Air 1150 °C
2100 °F
Upper limit of working range
Heatbath/Park Sta-Hard 45 Neutral Salt
A stable salt for neutral heating of ferrous and nonferrous alloys. Sta-Hard45 is similar to Sta-Hard 17, but provides higher working temperatures.Information provided by Heatbath Corporation - Park..
Maximum Service Temperature, Air 1150 °C
2100 °F
Skamol Group Skamol FL-06 Insulating Mortar
SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad..
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Unifrax Anchor-Loc® 2200 Ceramic Fiber Modules
The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us..
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Unifrax Anchor-Loc®2 2200 Ceramic Fiber Modules
Anchor-Loc®2 ceramic fiber modules extend the successful performance of standard Anchor-Loc folded modules to a product form featuring laminated fiber blanket constructin. This product combines ad..
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Unifrax Fibermass® 2200 Ceramic Fiber Blocks
Fibermass® ceramic fiber blocks combine advancements in fiber chemistry and manufacturing technology to provide an economical lining material for a wide range of heat processing equipment. The Fib..
Maximum Service Temperature, Air 1150 °C
2100 °F
CeramTec Rubalit® 600 Alumina, 48%
Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors.
Maximum Service Temperature, Air 1150 °C
2100 °F
Thermal Ceramics 2100 RPC Shapes
RPC 2100 is an economical insulating material produced by blending kaolin based alumino-silicate fibers with high purity silica fibers. The high temperature capability is enhanced by employing ammon..
Maximum Service Temperature, Air 1150 °C
2100 °F
Thermal Ceramics Kaowool 333-E Paper
Kaowool 333-E expandable paper is an intumescent material produced from a unique blend of Kaowool high-purity ceramic fibers, special additives, and organic binders in a special paper-making process..
Maximum Service Temperature, Air 1150 °C
2100 °F
Thermal Ceramics Superwool 612 Board
Superwool boards are processed from a slurry consisting of Superwool bulk and organic binders. Each board has cut edges for controlled squareness and trueness. Boards up to 36” wide may be ordered ..
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Duraboard® HD Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Maximum Service Temperature, Air 1149 °C
2100 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Maximum Service Temperature, Air 1150 °C
2100 °F
Universal Wire Works 117 Nickel Alloy Welding Wire
Alloy 117 is a nickel alloy electrode for welding nickel-chromium-cobalt-molybdenum alloys (UNS # N06617). This alloy electrode provides optimum strength and oxidation resistance above 1500 degrees ..
Maximum Service Temperature, Air 1150 °C
2100 °F
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate
Good mechanical strength, and electrical and thermal resistance. For producing insulators, standoffs, feed-thrus, furnace carriers and brazing fixtures. Fabricate and fire yourself using conventio..
Maximum Service Temperature, Air 1149 °C
2100 °F
BNZ Materials Bazelite 2000 Insulating Castable
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i..
Maximum Service Temperature, Air 1150 °C
2100 °F
Recommended Operating Temperature
Unifrax Fiberfrax® 880 Ceramic Fiber Paper
880 paper is made from a higher alumina content, shorter, smaller diameter fiber and laid up at higher densities. These product parameters lead to reduced shrinkage, higher strength, an increased o..
Maximum Service Temperature, Air 1150 °C
2100 °F
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy
Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at..
Maximum Service Temperature, Air 1149 °C
2100 °F
BNZ Materials Bazelite 2100 Insulating Castable
Blazelite 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting,..