Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.256 g/cc | 0.00925 lb/in³ | |
Pyrotek I-14 Insulating Board Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.A.. |
|||
Density | 0.256 g/cc | 0.00925 lb/in³ | |
Pyrotek MT-29Q Quilted Microporous Insulation MT-29Q is quilted to encapsulate its microporous core between glass cloth. The result is a flexible insulating material which offers exceptionally low thermal conductivity. The quilting maintains .. |
|||
Density | 0.256 g/cc | 0.00925 lb/in³ | |
Pyrotek O1-C Fiber Seal Pre-cut Gasket Silicone coated felt. Excellent resistance to vibration. Coating burns off at 315°C.Information provided by Pyrotek. |
|||
Density | 0.256 g/cc | 0.00925 lb/in³ | |
Pyrotek O-1C Low-Temperature Felt O-1 with a red silicone coating.Dimensions1524 mm x 22.9 m 6, 13, 25 mm thickApplicationsSiphon, air collection system, and carbon bake seals Makes an excellent air-tight, abrasion resistant seal In.. |
|||
Density | 0.256 g/cc | 0.00925 lb/in³ | |
Pyrotek MT-29L Microporous Ladle Lining Insulation MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the bac.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Installed Wet |
Unifrax Foamfrax® Grade I Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Installed Wet |
Unifrax Foamfrax® Grade II Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Installed Wet |
Unifrax Foamfrax® Grade III Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Installed Fired |
Unifrax Foamfrax® HD Grade I Fiber HD Insulation Foamfrax® HD Insulation is a monolithic thermal management product developed by Unifrax Corporation. This product is a four-component system of specially conditioned bulk ceramic fibers, an inorga.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Installed Fired |
Unifrax Foamfrax® HD Grade II Fiber HD Insulation Foamfrax® HD Insulation is a monolithic thermal management product developed by Unifrax Corporation. This product is a four-component system of specially conditioned bulk ceramic fibers, an inorga.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Installed Wet |
Unifrax Foamfrax® Isofoam Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Nominal |
Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | |
Hexcel® HexWeb® HDC - 3/16 - 16.0 (R2) Heavy Density Core Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with eit.. |
|||
Density | 0.256 g/cc | 0.00925 lb/in³ | ASTM D3574 |
3M 4108 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Density | 0.256 g/cc | 0.00925 lb/in³ | foam with adhesive; ASTM D3574 |
3M 4108 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | |
Unifrax Fiberfrax® 882-H Ceramic Fiber Paper This product is completely free of organics and used when higher fired strength is required or in processes and applications where even small amounts of organic burnout is unacceptable. 882-H has h.. |
|||
Density | 0.256 g/cc | 0.00925 lb/in³ | |
Pyrotek O-1 Low-Temperature Felt Excellent resistance to vibration. Not effected by 1.55 MPa steam.Dimensions1524 mm x 22.9 m 6, 13, 25 mm thickApplicationsHigh-density gaskets at elevated temperatures Initial systems, high pressu.. |
|||
Density | 0.256 g/cc | 0.00926 lb/in³ | Nominal |
Unifrax Fiberfrax® Duraboard® RG Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |