Material Notes:
Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application by caulking, troweling, or hand forming. Both products adhere well to most surfaces. Drying is accomplished at a noncritical, elevated temperature, and the resulting dried material is strong, hard, and erosion resistant. LDS-AL moldable possesses excellent resistance to wetting by many nonferrous molten metals and is used extensively in molten aluminum contact applications.Typical ApplicationsPatch refractory joints and cracksHardware protection of ceramic fiber furnace liningsPatch around burner blocksRefractory backupInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.801 g/cc
0.0289 lb/in³
Dry
1.36 g/cc
0.0492 lb/in³
Wet
Solids Content 55 %
55 %
Loss On Ignition 5.0 %
5.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00276 GPa
0.400 ksi
Dry
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1093 °C
1999 °F
Recommended Operating Temperature
Shrinkage 4.0 %

@Temperature 1090 °C,
Time 86400 sec
4.0 %

@Temperature 1990 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Appearance Sticky putty
Molten Aluminum Wetting Resistance Good
Temperature Grade (°F) 2300