Mechanical Properties Metric English Comments
Modulus of Rupture 0.00276 GPa
0.400 ksi
Imerys KT-Cast/Rogersâ„¢ Kaolin
Information provided by Imerys
Modulus of Rupture 0.00276 GPa
0.400 ksi
Dry
Unifrax Fiberfrax® LDS Moldable Moldable Insulation
Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b..
Modulus of Rupture 0.00276 GPa
0.400 ksi
Dry
Unifrax Fiberfrax® Pumpable-LDS Pumpable Insulation
Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have te..
Modulus of Rupture 0.00276 GPa
0.400 ksi
Zircar Ceramics AX Moldable Alumina-Silica Insulation
AX Moldable is a sticky fiber rich paste useful to obtain a hard surface coating, bond alumina-silica fiber based insulation products to themselves and to form complex shapes for use to 1260°C (230..