Material Notes:
Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527
Elongation at Break >= 200 %
>= 200 %
ISO 527
Flexural Modulus 1.05 GPa
152 ksi
ISO 178
Charpy Impact, Notched 0.130 J/cm²

@Temperature -20.0 °C
0.619 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75
Vicat Softening Point 130 °C
266 °F
ISO 306
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Users viewing this material also viewed the following: