Material Notes:
High-impact nylonInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm

@Thickness 3.20 mm
0.022 in/in

@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.024 cm/cm

@Thickness 3.20 mm
0.024 in/in

@Thickness 0.126 in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
ISO 527-1/-2
Elongation at Break >= 200 %
>= 200 %
ISO 527-1/-2
Tensile Modulus 0.800 GPa
116 ksi
ISO 527-1/-2
Flexural Strength 25.0 MPa
3630 psi
ISO 178
Flexural Modulus 0.800 GPa
116 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179-1
Charpy Impact, Notched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-2