Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 25.0 MPa | 3630 psi | STN EN ISO 178 |
Plastcom PLASTALEN® PC 69 T 10 003/1M Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | STN EN ISO 178 |
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Flexural Strength | 25.0 MPa | 3630 psi | |
Plastcom SLOVALEN PC 91 C 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C depending on th.. |
|||
Flexural Strength | <= 25.0 MPa | <= 3630 psi | ISO 178 |
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 25.0 MPa | <= 3630 psi | ISO 178 |
Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
SABIC B5429/B5429A High Density Polyethylene for Blow Molding Product Description: B5429 Series grades are medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades.. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
SABIC CC862 High Density Polyethylene for Injection Molding Product Description: SABIC HDPE CC862 is a high density polyethylene specially developed for still water bottle caps that meet organoleptic properties requirements. The material offers and ideal c.. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt .. |
|||
Flexural Strength | >= 25.0 MPa | >= 3630 psi | |
MarkeTech Repton EXP 386 Aluminum Titanate REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
LG Chemical LUPOL TE-5202U Thermoplastic Elastomer Alloy, 20% Polymer Alloy, High Impact, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | |
SPS Guang Zhou POPTREEâ„¢ 6001A Flame-retarded Polyethylene Characteristic: Low density, medium melt flow index, medium notched impact strength, no bloomingApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | |
SPS Guang Zhou SAMATâ„¢ 5000C Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high impact, high heat resistance, meets the requirements of RoHs and PaHsApplications: E/E applianceInformation Provided by.. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ISO 178 |
Unitika ET2025 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C10L Calcium Reinforced |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437M30CL Mica Reinforced Coupled |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ISO Data |
BASF Ultramid® 8202 HS PA6 (Conditioned) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Strength | 25.0 MPa @Temperature 65.0 °C |
3630 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Flexural Strength | 25.0 MPa @Temperature 65.0 °C |
3630 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Flexural Strength | 25.0 MPa @Temperature 120 °C |
3630 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C40L1 Calcium Reinforced |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436W20L Wollastonite Reinforced |
|||
Flexural Strength | 25.0 MPa | 3630 psi | STN EN ISO 178 |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | ASTM D790 |
Polyram RamOfin PPC300S4BK10 Polypropylene, 20% Glass beads 20% glass beads reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 25.0 MPa | 3630 psi | |
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |