Material Notes:
Universal 70S-6 is designed for welding mild steels with CO2 shielding gas. This alloy should be used where low silicon mild steel wires have not been satisfactory on slightly contaminated base metals. The additions of manganese and silicon deoxidizers improves the weld soundness and impact properties of this alloy using CO2 shielding gas. Excellent for use in standard MIG, semi-automatic, and automatic applications.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 517 MPa
75000 psi
Tensile Strength, Yield 434 MPa
63000 psi
Elongation at Break 28 %
28 %
Charpy Impact 31.2 J

@Temperature -28.9 °C
23.0 ft-lb

@Temperature -20.0 °F
67.8 J

@Temperature -17.8 °C
50.0 ft-lb

@Temperature 0.000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.090 %
0.090 %
Iron, Fe 97.3 %
97.3 %
As Remainder
Manganese, Mn 1.6 %
1.6 %
Phosphorous, P 0.015 %
0.015 %
Silicon, Si 0.95 %
0.95 %
Sulfur, S 0.020 %
0.020 %