Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 67.8 J @Temperature -17.8 °C |
50.0 ft-lb @Temperature 0.000 °F |
|
Universal Wire Works 70S-6 Steel Welding Wire Universal 70S-6 is designed for welding mild steels with CO2 shielding gas. This alloy should be used where low silicon mild steel wires have not been satisfactory on slightly contaminated base meta.. |
|||
Charpy Impact | 67.8 J @Treatment Temp. 1070 °C |
50.0 ft-lb @Treatment Temp. 1950 °F |
austenitized; C-notch |
Crucible Steel CPM® 4V® Tool Steel CPM 4V is a powder metal tool steel with an outstanding combination of properties including high impact toughness and very good wear resistance. CPM 4V should be considered for service in fine blank.. |
|||
Charpy Impact | 67.8 J @Tempering Temp. 482 °C |
50.0 ft-lb @Tempering Temp. 900 °F |
hardened at 1800°F then tempered; C-notch |
Crucible Steel CRUCIBLE A9 Tool Steel Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the .. |
|||
Charpy Impact | 67.8 J @Tempering Temp. 510 °C |
50.0 ft-lb @Tempering Temp. 950 °F |
hardened at 1800°F then tempered; C-notch |
Crucible Steel CRUCIBLE A9 Tool Steel Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the .. |
|||
Charpy Impact | 67.8 J @Treatment Temp. 1040 °C |
50.0 ft-lb @Treatment Temp. 1900 °F |
Solution Treated; V-notch |
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
Charpy Impact | 67.8 J @Tempering Temp. 593 °C |
50.0 ft-lb @Tempering Temp. 1100 °F |
oil quenched from 1525°F then tempered |
Crucible Steel Holder Block Steel, AISI 4150 Modified Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b.. |
|||
Charpy Impact | 67.8 J @Temperature -73.3 °C |
50.0 ft-lb @Temperature -100 °F |
Transverse |
ATI Allegheny Ludlum AL 412™ Dual Phase 12% Cr Low carbon, nickel containing, dual phase 12% Cr stainless steel alloy. Characteristics: superior toughness to ferritic alloys, high strength, high corrosion resistance.Information provided by Alleg.. |