Universal Wire Works Inconel 62 (AMS 5679) Nickel Alloy Filler Metal

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works Inconel 62 (AMS 5679) Nickel Alloy Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Inconel Filler Metal 62 is a nickel chromium alloy designed for welding nickel base alloy 600 in up to 2" thicknesses using the gas tungsten arc, gas metal arc and submerged arc processes. Filler Metal 82 is recommended for sections exceeding 2".Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 16 %
16 %
Cobalt, Co 0.10 %
0.10 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe 8.0 %
8.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nb + Ta 2.0 %
2.0 %
Nickel, Ni 71 %
71 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.35 %
<= 0.35 %
Sulfur, S <= 0.015 %
<= 0.015 %