Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Von Roll Isola IMI E-Solder® 3025 Electrically Conductive Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Von Roll Isola
Trade Name IMI E-Solder®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Von Roll Isola IMI E-Solder® 3025 Electrically Conductive Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue to contaminate sensitive electronic components.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.0 MPa
2470 psi
butt tensile strength per ASTM D426 on brass
Adhesive Bond Strength 14.0 MPa
2030 psi
Tensile shear per ASTM D1002 on etched Al panel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0400 ohm-cm
0.0400 ohm-cm
cured 24 hr at 25°C (77°F). Value is 0.004 Ohm-cm cured 3 hr at 65°C (150°F)
Processing Properties Metric English Comments
Processing Temperature 65.0 °C
149 °F
Suggested baking time at this temperature is 4 hr.
Users viewing this material also viewed the following: