Mechanical Properties Metric English Comments
Adhesive Bond Strength 14.0 MPa
2030 psi
Phenolic, Shear; ISO 4587
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Adhesive Bond Strength >= 14.0 MPa
>= 2030 psi
Acrylic, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength 14.0 MPa
2030 psi
Phenolic, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength <= 14.0 MPa
<= 2030 psi
Steel to Ferrite, Substrate Failure, Shear
Permabond ES550 Epoxy Resin
PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
Permabond ES550 Epoxy Resin
PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng..
Adhesive Bond Strength 14.0 - 41.0 MPa
2030 - 5950 psi
Zinc, Shear; ASTM D1002
Permabond ES558 Epoxy Resin
PERMABOND ES558 is a single-part epoxy paste which flows like solder when heated during curing. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear strength...
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Aluminum, Shear; ISO 4587
Permabond ES562 Epoxy Resin
PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ISO 4587
Permabond ES562 Epoxy Resin
PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
Permabond ES578 Epoxy Resin
PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon..
Adhesive Bond Strength 14.0 MPa
2030 psi
steel collar and pin shear; ISO 10123
Permabond HM160 Anaerobic Retaining Compound
Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces..
Adhesive Bond Strength >= 14.0 MPa
>= 2030 psi
Substrate Failure, Steel to Ferrite using Initiator 41 after 24 hours, Shear
Permabond TA437 Toughened Acrylic Adhesive
PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –..
Adhesive Bond Strength 14.0 - 20.0 MPa
2030 - 2900 psi
Mild steel, Shear
Permabond TA437 Toughened Acrylic Adhesive
PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –..
Adhesive Bond Strength >= 14.0 MPa
>= 2030 psi
Substrate Failure, Steel to Ferrite after 24 hours, Shear
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
Adhesive Bond Strength >= 14.0 MPa
>= 2030 psi
Ferrite/steel after 24 hours, Shear
Permabond TA459 Toughened Acrylic Adhesive
Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens..
Adhesive Bond Strength >= 14.0 MPa
>= 2030 psi
Ferrite/steel after 24 hours, Shear
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..
Adhesive Bond Strength >= 14.0 MPa
>= 2030 psi
Substrate Failure, Steel to Ferrite, after 24 hours, Shear
Permabond TA4592 Toughened Acrylic Adhesive
PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt..
Adhesive Bond Strength 14.0 - 17.0 MPa
2030 - 2470 psi
Glass/steel, Shear
Permabond UV7141 UV-curable Adhesive
Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet..
Adhesive Bond Strength 14.0 MPa
2030 psi
Phenolic, Shear; ISO 4587
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
Adhesive Bond Strength 14.0 MPa
2030 psi
Phenolic, Shear; ISO 4587
Permabond 919 Cyanoacrylate, High temperature
Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I..
Adhesive Bond Strength 14.0 MPa
2030 psi
Phenolic, Shear; ISO 4587
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..
Adhesive Bond Strength 14.0 MPa
2030 psi
steel collar and pin shear; ISO 10123
Permabond HH040 Anaerobic Retainer
Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz..
Adhesive Bond Strength 14.0 MPa
2030 psi
steel collar and pin shear; ISO 10123
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer
Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u..
Adhesive Bond Strength 14.0 MPa
2030 psi
Tensile shear per ASTM D1002 on etched Al panel
Von Roll Isola IMI E-Solder® 3022 Electrically Conductive Adhesive
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t..
Adhesive Bond Strength 14.0 MPa
2030 psi
Varies with substrates
Loctite® 3273 Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Adhesive Bond Strength 14.0 MPa
2030 psi
Tensile shear per ASTM D1002 on etched Al panel
Von Roll Isola IMI E-Solder® 3012 Electrically Conductive Adhesive
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t..
Adhesive Bond Strength >= 14.0 MPa
>= 2030 psi
Acrylic, Shear; ISO 4587
Permabond 910FS Cyanoacrylate, Methyl grade
PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts..
Adhesive Bond Strength 14.0 MPa
2030 psi
Tensile shear per ASTM D1002 on etched Al panel
Von Roll Isola IMI E-Solder® 3025 Electrically Conductive Adhesive
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t..
Adhesive Bond Strength 14.0 MPa

@Temperature 25.0 °C
2030 psi

@Temperature 77.0 °F
Tensile Lap Shear
Henkel Hysol EA 9825 Paste Adhesive System
Low-density, one-component epoxy syntactic for use on honeycomb composite parts requiring high compressive strength at temperatures up to 350°F / 177°C. Ideal for fastener or attachment potting an..