Wall Colmonoy COLMONOY® 23A & 24 - Nickel Alloy With Tungsten Carbide

Category Metal , Metal Matrix Composite , Nonferrous Metal , Nickel Alloy , Tungsten Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name COLMONOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy COLMONOY® 23A & 24 - Nickel Alloy With Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description and Application: Used to repair blow holes, flaws, chips, and cracks in cast iron parts. No. 23A works best in repairing surface flaws, No. 24 is recommended for working on edges or corners. Finished by grinding or filing.Method of Application: Fusewelder Information provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 8.64 g/cc
0.312 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 16 - 23
16 - 23
Component Elements Properties Metric English Comments
Boron, B 1.5 %
1.5 %
Carbon, C 0.020 %
0.020 %
Chromium, Cr 0.080 %
0.080 %
Iron, Fe 0.12 %
0.12 %
Nickel, Ni 95.78 %
95.78 %
As Balance
Silicon, Si 2.5 %
2.5 %
Processing Properties Metric English Comments
Processing Temperature 1070 °C
1950 °F
fusing temperature