Wanshijie APET Sheet

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Wanshijie Plastic Sheet Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanshijie APET Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APET sheet is one of the earliest plastic sheets our company develops and produces. It has excellent air-tightness, durability, chemical resistance and transparency. When burnt, it will not produce any toxic gas, so it is environment friendly. Also it complies with American FDA and Japanese food safety standard. It has become the safety material for foodstuff. In addition, it is applicable for various machining, displaying or exhibiting, vacuum forming and etc.GOOD TRANSPARENCY: It has above 87 percent of transparency and good texture touch and is suitable for the products that require high transparency.EXCELLENT IMPACT STRENGTH RESISTANCE AND RIGIDITY: Hard and durable material, good physical property even at 40°C,suitable for the products that require high Impact strength resistance.EXCELLENT THERMOFORMING: Be able to form when preheating is not needed, high precision, about 0.5 percent shrinkage, excellent deep thermoforming, even thickness and no crack.EXCELLENT FOOD SAFETY: APET material can comply with all main food regulations, such as FDA or BGA. Suitable for food container packing.EXCELLENT GREASE AND CHEMICAL RESISTANCE: No corrosion to acid, alkali, oil and etc.LOW COMBUSTIBILITY: Excellent fire resistance, no support combustion, less smoke, no harmful substances after combustion.ENVIRONMENT PROTECTION: Available to recycle and no environment pollution.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D1050
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 52.4 MPa
7600 psi
ASTM D638
Film Tensile Strength at Yield, TD 53.0 MPa
7690 psi
ASTM D638
Elongation at Yield 266 %
266 %
ASTM D638
Modulus of Elasticity 2.20 GPa
319 ksi
ASTM D638
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Thermal Properties Metric English Comments
Heat Distortion Temperature 75.0 °C
167 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 87 %
87 %
ASTM D1003
Users viewing this material also viewed the following: