Material Notes:
Homopolymer. Meets GMP.PP.030 spec.Applications: Fan shrouds, heater housings, various under hood uses.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
8-12 g/10min; Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 2.70 GPa
392 ksi
Secant; ASTM D790
Izod Impact, Notched 0.400 J/cm

@Thickness 3.17 mm
0.749 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
ASTM D648