Weartech International WT-25 Cobalt Hardfacing & Wear Resistant Alloy

Category Metal , Nonferrous Metal , Cobalt Alloy
Manufacturer Weartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Weartech International WT-25 Cobalt Hardfacing & Wear Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Weartech International
Physical Properties Metric English Comments
Density 9.13 g/cc
0.330 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 16 - 24
16 - 24
Tensile Strength 1070 MPa
155000 psi
Heat Treated
Charpy Impact >= 8.13 J
>= 6.00 ft-lb
Thermal Properties Metric English Comments
CTE, linear 16.4 µm/m-°C
9.10 µin/in-°F
Specific Heat Capacity 0.385 J/g-°C
0.0920 BTU/lb-°F
Melting Point <= 1410 °C
<= 2570 °F
Liquidus 1410 °C
2570 °F
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 20 %
20 %
Cobalt, Co 50.9 - 53.9 %
50.9 - 53.9 %
Iron, Fe <= 3.0 %
<= 3.0 %
Nickel, Ni 10 %
10 %
Silicon, Si 1.0 %
1.0 %
Tungsten, W 15 %
15 %