Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman EcoLon® MRGF1878-BK1 Nylon 6, 30% Mineral/Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name EcoLon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman EcoLon® MRGF1878-BK1 Nylon 6, 30% Mineral/Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.011 cm/cm
0.0070 - 0.011 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
ISO 527-93
Elongation at Break 2.0 %
2.0 %
ISO 527-93
Flexural Strength 150 MPa
21800 psi
ISO 178-93
Flexural Modulus 7.10 GPa
1030 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-93