Material Notes:
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties allow engineers and designers the ability to create cost-effective, innovative parts that exhibit outstanding wear, heat, electrical and chemical resistance. The TECAPEEK™ family is made up of materials for medical applications.TECAPEEK™ MT, unfilled pigmented medical grade PEEKTECAPEEK™ XP98, compression molded 30% carbon fiber filled PEEK (isotropic properties)TECAPEEK™ MT CF30, extruded 30% carbon fiber filled PEEKTECAPEEK™ Classic™, ISO 10993 certification by resin and extrusion lot of 30 days contactTECAPEEK™ Classix™ XRO-20 radio opaque grade with 20% BaSO4 addedThe TECAPEEK™ family of high performance plastics are high effective in the creation and manufacture of high quality medical instruments. Five separate grades, each with qualities to meet a wide range of requirements for the engineer and product designer.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
ASTM D792
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa

@Temperature 22.8 °C
11600 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 5.00 GPa

@Temperature 22.8 °C
725 ksi

@Temperature 73.0 °F
1% Secant; ASTM D638
Flexural Modulus 4.00 GPa

@Temperature 22.8 °C
580 ksi

@Temperature 73.0 °F
ASTM D790
Thermal Properties Metric English Comments
Melting Point 340 °C
644 °F
Maximum Service Temperature, Air 260 °C
500 °F
continuous