Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.50 - 3.50 kJ/m² @Temperature -30.0 - -30.0 °C |
1.67 - 1.67 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.50 kJ/m² Grade Count:1 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched (ISO) | 3.50 - 17.0 kJ/m² @Temperature -40.0 - -20.0 °C |
1.67 - 8.09 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 8.86 kJ/m² Grade Count:31 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FPT 20 - 20% Talc Reinforced Polypropylene Homopolymer Compound 20% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66 Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman EcoLon® MR1660-BK1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF13-66 22LH-NBK1 13% Glass Fiber Reinforced, General Purpose Nylon 66 Description: Glass Fiber Reinforced, General Purpose Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® MR410 22H-WBK 40% Mineral Reinforced, Weatherable Black Nylon 66 Description: Mineral Reinforced, Weatherable Black Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® MRGF3820-N 38% Mineral/Glass Reinforced Developmental Grade Nylon 66 Description: Mineral/Glass Reinforced Developmental Grade Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180 |
Total PPH 12020 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min.Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transpa.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 7059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning propert.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 7060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7060 is homopolymer.ApplicationATOFINA Polypropylene PPH 7060 is intended for the injection molding of packaging containers, toys, domestic appliances, garden furniture and.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 9089 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9089 is a very low molecular weight distribution homopolymer propylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9089 is intended for the ex.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 9099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9099 is a very narrow molecular weight distribution homopolymer polypropylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9099 is intended for.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180 |
Total PPM H250 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H250 is a narrow molecular weight distribution homopolymer with a Melt Flow Index of 25 g/10 min recommended for the manufacture of medical packaging and medical devices, to the ex.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® PP FR V0 - UL94-V0 Flame Retardant Polypropylene Homopolymer V-0 Flame Retardant PP HomopolymerApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO-180 |
Diamond Polymers SBS 1001 Styrene Butadiene Block Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness >=5.00 mm |
1.67 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 542 Polypropylene Homopolymer Unreinforced, high heat resistance, antistaticInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 560 Polypropylene Homopolymer High heat resistance, detergent stabilized, anti-yellowingInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl A2 G30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -30.0 °C |
1.67 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® C3U PA66/6 (Dry) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
Izod Impact, Notched (ISO) | 3.50 - 7.00 kJ/m² | 1.67 - 3.33 ft-lb/in² | Average value: 4.79 kJ/m² Grade Count:14 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, Conditioned Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 G30 Nylon 6, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Qualchem Danamid FGFTALX2-5 20 Polyamide 6, 25% Glass Fiber Reinforced with glass fiber and minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |