Westlake EC479AA Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EC479AA Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
WESTLAKE low-density polyethylene EC479 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Application/UsesFolded cartonsFlexible packagingCupsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.9215 g/cc
0.03329 lb/in³
ASTM D1505
Melt Flow 5.7 g/10 min
5.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 475 %
475 %
ASTM D638
Tensile Modulus 0.138 GPa
20.0 ksi
ASTM D1709
Processing Properties Metric English Comments
Melt Temperature 302 - 329 °C
575 - 625 °F
Descriptive Properties Value Comments
Process Coating
Region US & Canada
Bamberger Polymers Distribution