Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows Processing Temperature Range of 280-600°F; Non-corrosive at all Temperature Ranges; No FDA Thickness Limitations; Contains a High Level of Slip and Antiblock AdditivesApplications:Film: Excellent Heat Seal Response at Low Temperatures, Making it a Good Candidate for the Heat Seal Layer in Various Coextrusion Constructions; Coatings & Laminations: Higher Neck-In but Similar Drawdown vs. Polyethylene, Excellent Heat Seal Response at Low Seal Temperatures, Processing Temperature Range - 580-600°F, Can be Drawn as Low as 4 lbs. per ream, Gas Barrier and Grease Resistance are Slightly Less than those of LDPE; Coextrusion: Excellent Coextrusion Tie Layer for LDPE, LLDPE, HDPE, PP, EVA, EEA, Ionomer, PET, PC, PVDC and rigid PVC; Injection Molding: Processing Temperature 360-600°F, Less Mold Shrinkage than LDPE, Produces Very Tough, Stress Crack Resistant PartsEastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D1505
ESCR 10% Igepal® >= 360 hour

@Temperature 50.0 °C
>= 360 hour

@Temperature 122 °F
F<sub>50</sub>; ASTM D1693
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Cond. E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Hardness, Shore D 31
31
ASTM D2240
Tensile Strength, Ultimate 11.4 MPa
1650 psi
ASTM D638
Elongation at Break 750 %
750 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 82.0 °C
180 °F
by DSC
Vicat Softening Point 58.0 °C
136 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 154 °C
309 °F
Blown Film
190 °C
374 °F
Molding
315 °C
599 °F
Extrusion Coating