Physical Properties Metric English Comments
ESCR 10% Igepal® >= 360 hour

@Temperature 50.0 °C
>= 360 hour

@Temperature 122 °F
F<sub>50</sub>; ASTM D1693
Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer  (discontinued **)
20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to ..
ESCR 10% Igepal® >= 360 hour

@Temperature 50.0 °C
>= 360 hour

@Temperature 122 °F
F<sub>50</sub>; ASTM D1693
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer  (discontinued **)
20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows ..
Copyright © lookpolymers.com All Rights Reserved