Westlake LF2020 Hexene Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake LF2020 Hexene Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake LF2020 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include stretch films, heavy duty bags and sacks, agricultural films, and trash bags & liners. This Kosher compliant material is available with various slip and antiblock levels.Application/UsesBags and sacksAgricultural filmsTrash bags and linersCo-extruded structuresFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 670 %
670 %
ASTM D882
Film Elongation at Break, TD 900 %
900 %
ASTM D882
Dart Drop 8.66 g/micron
220 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 40.7 MPa
5900 psi
ASTM D882
Film Tensile Strength at Break, TD 28.3 MPa
4100 psi
ASTM D882
1% Secant Modulus, MD 207 MPa
30000 psi
ASTM D882
1% Secant Modulus, TD 248 MPa
36000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 204 - 216 °C
400 - 420 °F
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution