Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer Westlake Plastics
Trade Name Norylux™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most dimensionally stable thermoplastics available. It is used for a variety of structural applications including electrical housings, scientific instrumentation parts, and fluid handling components. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D7852
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Yield Strength 99.3 MPa
14400 psi
ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 59.4 µm/m-°C

@Temperature 20.0 °C
33.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
254 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0580 in
Electrical Properties Metric English Comments
Dielectric Constant 2.69

@Frequency 60 Hz
2.69

@Frequency 60 Hz
ASTM D150
Dielectric Strength 50.0 kV/mm
1270 kV/in
ASTM D149
Dissipation Factor 0.00070

@Frequency 60 Hz
0.00070

@Frequency 60 Hz
ASTM D150