Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 30% Glass Filled
Manufacturer Westlake Plastics
Trade Name Norylux™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most dimensionally stable thermoplastics available. It is used for a variety of structural applications including electrical housings, scientific instrumentation parts, and fluid handling components. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell L 108
108
ASTM D7852
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
285 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0580 in
Electrical Properties Metric English Comments
Dielectric Constant 3.15

@Frequency 60 Hz
3.15

@Frequency 60 Hz
ASTM D150
Dielectric Strength 53.0 kV/mm
1350 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 60 Hz
0.0020

@Frequency 60 Hz
ASTM D150