Westlake Plastics Tempalux® CN-F Polyetherimide (conductive)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer Westlake Plastics
Trade Name Tempalux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Tempalux® CN-F Polyetherimide (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resistance and excellent fabrication finishing characteristics. UL94 V-0 rated. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Water Absorption 0.45 %
0.45 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 92
92
ASTM D2240
Tensile Strength, Yield 200 MPa
29000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 262 MPa
38000 psi
ASTM D790
Flexural Modulus 12.8 GPa
1860 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
417 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0580 in
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm - 1e+05
10000 ohm-cm - 1e+05
Dry; ASTM D257
Surface Resistance 10000 ohm - 1e+05
10000 ohm - 1e+05
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B