Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1860 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.8 GPa
1860 ksi
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability
FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo..
Flexural Modulus 12.8 GPa

@Temperature 23.0 °C
1860 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB SCANMID 6 B11^ F45 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Modulus 12.8 GPa

@Temperature 23.0 °C
1860 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB SCANMID 6 B12^ F45 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Modulus 12.8 GPa
1860 ksi
ASTM D790
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Flexural Modulus 12.8 GPa
1860 ksi
5 mm/min; ISO 178
Gromax BFG50-BN00N1 Nylon 6 60% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Flexural Modulus 12.8 GPa
1860 ksi
2 mm/min; ISO 178-A
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral
PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS.
Flexural Modulus 12.8 GPa
1860 ksi
ASTM D790
Plenco 5350 Phenolic, Granular, Injection Molded
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties...
Flexural Modulus 12.8 GPa
1860 ksi
ASTM D790
Westlake Plastics Tempalux® CN-F Polyetherimide (conductive)
Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resist..
Flexural Modulus 12.8 GPa
1860 ksi
ASMT D790
Toyobo TS401 PPS, 40% Glass Fiber Reinforced
Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec..
Flexural Modulus 12.8 GPa
1860 ksi
ISO 178
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized
Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Flexural Modulus 12.8 GPa
1860 ksi
ISO Data
BASF Petra® 140 BK-112 45% Glass Filled PET
Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa..
Flexural Modulus 12.8 - 13.6 GPa
1860 - 1970 ksi
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester
BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i..
Flexural Modulus 12.8 GPa
1860 ksi
ASTM D790
Plenco 7552 Phenolic, Nodular, Transfer Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..