Wieland 1408 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1408 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hard yellow gold alloy. Easily splintered and polished.Applications: casting, laminar decoration, tubingDental
Physical Properties Metric English Comments
Density 13.8 g/cc
0.499 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 170
170
HV5; glowed
Tensile Strength, Ultimate 550 MPa
79800 psi
Elongation at Break 30 %
30 %
Thermal Properties Metric English Comments
Melting Point 830 - 850 °C
1530 - 1560 °F
Solidus 830 °C
1530 °F
Liquidus 850 °C
1560 °F
Component Elements Properties Metric English Comments
Copper, Cu 16.1 %
16.1 %
Gold, Au 58.5 %
58.5 %
Silver, Ag 25 %
25 %
Zinc, Zn 0.40 %
0.40 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 950 - 1050 °C
1740 - 1920 °F
Descriptive Properties Value Comments
Color yellow 1N