Wieland Portalloy 54 PFM Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Palladium Alloy
Manufacturer Wieland
Trade Name Portalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Portalloy 54 PFM Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental
Physical Properties Metric English Comments
Density 13.8 g/cc
0.499 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 260
260
HV5/30; after porcelain firing
280
280
HV5/30; hardened
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
after porcelain firing
649.8 MPa

@Strain 0.200 %
94250 psi

@Strain 0.200 %
hardened
Elongation at Break 5.0 %
5.0 %
hardened
6.0 %
6.0 %
after porcelain firing
Modulus of Elasticity 120 GPa
17400 ksi
Thermal Properties Metric English Comments
CTE, linear 13.8 µm/m-°C

@Temperature 25.0 - 500 °C
7.67 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Gold, Au 54.2 %
54.2 %
Indium, In 9.0 %
9.0 %
Palladium, Pd 31 %
31 %
Silver, Ag 4.8 %
4.8 %
Processing Properties Metric English Comments
Processing Temperature 849 °C
1560 °F
Preheating Temp.
Melt Temperature 1100 - 1240 °C
2010 - 2270 °F
Casting Temperature 1400 °C
2550 °F
Descriptive Properties Value Comments
Color white