Processing Properties Metric English Comments
Casting Temperature 1400 °C
2550 °F
Wieland Duo Pal 6 PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Casting Temperature 1400 °C
2550 °F
Wieland Euro 50 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental
Casting Temperature 1400 °C
2550 °F
Wieland Portalloy 54 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental
Casting Temperature 1400 °C
2550 °F
Wieland Simidur KF Plus PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Casting Temperature 1400 °C
2550 °F
Wieland Simidur Superior PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental