Material Notes:
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Physical Properties Metric English Comments
Density 10.5 g/cc
0.379 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 300
300
HV5/30; after porcelain firing
350
350
HV5/30; hardened
Tensile Strength, Yield 640 MPa

@Strain 0.200 %
92800 psi

@Strain 0.200 %
after porcelain firing
800 MPa

@Strain 0.200 %
116000 psi

@Strain 0.200 %
hardened
Elongation at Break 14 %
14 %
hardened
22 %
22 %
after porcelain firing
Modulus of Elasticity 120 GPa
17400 ksi
Thermal Properties Metric English Comments
CTE, linear 13.8 µm/m-°C

@Temperature 25.0 - 500 °C
7.67 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Gallium, Ga 6.0 %
6.0 %
Indium, In 6.0 %
6.0 %
Palladium, Pd 79.7 %
79.7 %
Ruthenium, Ru 0.30 %
0.30 %
Silver, Ag 2.0 %
2.0 %
Tin, Sn 4.0 %
4.0 %
Zinc, Zn 2.0 %
2.0 %
Processing Properties Metric English Comments
Processing Temperature 849 °C
1560 °F
Preheating Temp.
Melt Temperature 1100 - 1260 °C
2010 - 2300 °F
Casting Temperature 1400 °C
2550 °F
Descriptive Properties Value Comments
Color white
Users viewing this material also viewed the following: