Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Williams Advanced Alloys WS179 Solder

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS179 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 8.41 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.0 MPa
6380 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 42.0 W/m-K
291 BTU-in/hr-ft²-°F
Melting Point 179 °C
354 °F
Solidus 179 °C
354 °F
Liquidus 179 °C
354 °F
Component Elements Properties Metric English Comments
Lead, Pb 36 %
36 %
Silver, Ag 2.0 %
2.0 %
Tin, Sn 62 %
62 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001445 ohm-cm
0.00001445 ohm-cm
Users viewing this material also viewed the following: