Material Notes:
Quenched and tempered for extreme abrasion and moderate impact.Winco-Tuf 40 has excellent toughness at high hardness and in heavy sections. For severe abrasions. Advantages: Maximum resistance to abrasion and impact.Withstands the brittleness which develops at subnormal temperatures.Increased toughness and fatigue resistance compared to low carbon and 1045 plate.Retains high strength and wearability at high temperatures.High impact and wear properties retained at weld joints.Information from Wingate Alloys Inc.
Mechanical Properties Metric English Comments
Hardness, Brinell 375 - 440
375 - 440
Hardness, Rockwell C 40 - 46
40 - 46
Tensile Strength 1380 MPa
200000 psi
Tensile Strength, Yield 1100 MPa
160000 psi
Elongation at Break 14.4 %
14.4 %
2[in]
Reduction of Area 55 %
55 %
Component Elements Properties Metric English Comments
Carbon, C 0.17 - 0.25 %
0.17 - 0.25 %
Chromium, Cr 0.45 - 0.60 %
0.45 - 0.60 %
Copper, Cu 0.15 - 0.30 %
0.15 - 0.30 %
Iron, Fe 95.21 - 96.33 %
95.21 - 96.33 %
Manganese, Mn 1.5 %
1.5 %
Molybdenum, Mo 0.20 - 0.60 %
0.20 - 0.60 %
Nickel, Ni 0.70 - 1.0 %
0.70 - 1.0 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S <= 0.015 %
<= 0.015 %