Zircar Ceramics AL-CEM Alumina Cement

Category Ceramic , Oxide , Aluminum Oxide , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Zircar Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Ceramics AL-CEM Alumina Cement.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type AL-CEM Alumina Cement is a high purity alumina bonding agent used for bonding ZIRCAR® fibrous ceramic products to themselves, and as a coating cement to improve the hardness and oxidation resistance of substrates. Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Density 1.95 g/cc
0.0704 lb/in³
Solids Content 70 %
70 %
Thermal Properties Metric English Comments
Melting Point >= 1870 °C
>= 3400 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Component Elements Properties Metric English Comments
Al2O3 99.2 %
99.2 %
SiO2 0.80 %
0.80 %
Descriptive Properties Value Comments
Color White
Coverage 7 ft2
1 Pint as 0.01" Layer on Fibrous Ceramic Insulation
Weight Per Pint 2 lbs