Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1649 °C | 3000 °F | |
Pyrotek REDLINE MULTIKOTE Water-Based Coating A water-based coating designed to prevent molten metal adhesion to both refractory and most metallic surfaces. Multikote's bonding system enables it to be applied in a variety of applications .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Pyrotek SP-160 Refractory Coating Blended with water SP-160 produces a hard, highly refractory coating for fibrous ceramic or metal shapes. It is an alumina bonded refractory coating system, thyrotrophic in nature which promotes go.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Pyrotek Pyrocast ICL Castable Refractory Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist.. |
|||
Maximum Service Temperature, Air | 1649 °C | 3000 °F | |
Pyrotek Pyrocast ZC Refractory Shapes Aggregate Base: MulliteApplicationsDoor sill Breech plug Door jamb Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Continuous |
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
GBC Grade 97 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
GBC Grade 98 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Sharadaa Ceramics HA 90SD High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Quick Immersion |
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | Quick Immersion |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Zircar Ceramics APA-2 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-2 is a flexible un-bonded sheet that contains no organic binder. Applications include thermal insulation in low .. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1650 °C | >= 3000 °F | |
China-Yixing Longly Refractories ZTA (10%ZrO2) Zirconia Toughened Alumina Composite Ceramic LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | limited |
Chosun Refractories TCH-175Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1649 °C | 3000 °F | Normal oxidizing atmosphere |
BNZ Materials BNZ-3000 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
BNZ Materials Super Blakbond Mortar Super Blakbond is an air-setting mortar for general purpose plant use. It has greater air-setting strength than Blakbond or No. 2986. It is good for insulating fire brick where greater bond strength.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabind™ 644-A High Temperature Inorganic Binder An acidic, colloidal alumina binder developed for mixing with sized refractory flours and grains to produce high temperature refractory coatings for ceramic fiber boards. Used as a superior standalo.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
BNZ Materials Blakbond Mortar Blakbond is a highly refractory mortar which possesses high water retention properties. It is especially designed for laying insulating fire brick and is also used for super duty and high alumina de.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURON 165 Dense Refractory Castable Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast CURON 165 GM Dense Refractory Castable Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo.. |
|||
Maximum Service Temperature, Air | 1650 °C | 3000 °F | |
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |