Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Zircar Refractory Composites, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conductivity and is designed for use in applications where purity, cracking resistance, high strength and resistance to heat are paramount. Due to its exceptional resistance to heat flow for its thickness, it provides maximum thermal resistance where space is at a premium. This material is virtually shot free and is the cleanest refractory paper available. It is ideal for applications up to 1260°C (2300°F). Type ASPA-2 is produced with no organic volatiles and will not produce smoke or odor when heated.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 0.128 g/cc
0.00462 lb/in³
Loss On Ignition <= 0.50 %
<= 0.50 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.0500 W/m-K

@Temperature 500 °C
0.347 BTU-in/hr-ft²-°F

@Temperature 932 °F
0.0800 W/m-K

@Temperature 800 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 1470 °F
0.130 W/m-K

@Temperature 871 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1600 °F
0.160 W/m-K

@Temperature 1100 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Component Elements Properties Metric English Comments
Al2O3 51 %
51 %
SiO2 49 %
49 %
Descriptive Properties Value Comments
Color White
Fiber Index, % 75
Mullen Burst, psi 20
Type of Binder none
Users viewing this material also viewed the following: