Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.160 W/m-K @Temperature 870 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Pyrotek M-14 Compressible/Insulating Boards ApplicationsSiphon gaskets Trough and ladle linings Tundishes Mill board substitute AdvantagesResistant to chemical attack Excellent thermal shock resistance Slightly flexible Moderately compressibl.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 540 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 538 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast L-30 Moldable Refractory Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommen.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 540 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast L-40 Insulating Refractory Pyrocast L-40 is a fiber free refractory moldable designed for use in contact with molten aluminum. L-40 has excellent workability for use as an insulating lining or patching material.Recommended C.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.160 - 0.240 W/m-K @Temperature 600 °C |
1.11 - 1.67 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be .. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group V-1100 600 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 600 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group V-LITE 375 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group V-LITE 475 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Ceramics AL-25/1700 Alumina Insulation AL-25/1700 is a rigid medium duty grade of alumina fiber board. Not as strong as SALI but capable of delivering years of service.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 1075 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1967 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 900 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 649 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Tritex TRI-F Blanket Insulation TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 1100 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 1100 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher .. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
parallel to thickness; ASTM C177 |
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE ZIRCAR Alumina-Silica Insulating Blanket Type RS-B Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped .. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 538 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-23A Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 204 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
BNZ Materials Marinite® P High Temperature Structural Insulation Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 1100 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |