Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 155 °C | 311 °F | NEMA temperature |
Glastic Laminates/Shapes UTS Fiberglass-Reinforced Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-2. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | Continuous |
Lord Adhesives Circalokâ„¢ 6031 A/B Epoxy Encapsulant Circalokâ„¢ 6031 A/B is a two-part epoxy potting compound with excellent electrical properties at elevated temperatures. Good arc-track resistance under high voltage loading and other dielectric .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | Continuous |
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 60216-1, Electric strength, 20000 h |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | Approximate temperature class |
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) This IEEE Class F 155ºC high strength material exhibits substantial resistance to cold flow or creep under heat and pressure. Suggested applications include motor slot wedges, washers, brush plat.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | UL temperature Index |
Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | UL temperature Index |
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | Heat Resistance; ASTM D570D |
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Von Roll Isola IMI Varnish 3255 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Von Roll Isola IMI Varnish 74011 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Von Roll Isola IMI Varnish 74035 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >99°C. Usa.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Von Roll Isola IMI Varnish 9522 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 24°C. Average solids: 50%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, bare copper coils, etc.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Zotefoams ZOTEK® F 40 HT LS PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Zotefoams ZOTEK® F 40 HT PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Eccobond® 11 Heat Cure Catalyst Emerson & Cuming 11 Eccobond® Heat Cure CatalystGeneral purpose, low viscosity, elevated temperature curing. Long working life. Yields cured coatings with excellent chemical resistance. Subject to .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Eccobond® 1962-31 Needle Bonding Epoxy Adhesive Emerson & Cuming 1962-31 Eccobond® Needle Bonding Epoxy AdhesiveOne component, medium viscosity, epoxy needle bonding adhesive. Designed to bond stainless steel cannulae into polypropylene hubs. Al.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Eccobond® A316-48 One-Component Fast Cure Epoxy Adhesive Emerson & Cuming A316-48 Eccobond® One-Component Fast Cure Epoxy AdhesivePourable, fast heat curing, epoxy adhesive and insulation compound. Excellent chemical and heat resistance. Cure Type: Heat .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 216 |
Dr. D. Mueller Flexiso® DMD FI 14010 00100 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00100 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 216 |
Dr. D. Mueller Flexiso® DMD FI 14010 00210 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00210 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 216 |
Dr. D. Mueller Flexiso® DMD FI 14010 00460 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00460 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Cytec (Conap) FR-1046 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Cytec (Conap) FR-1047 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Cytec (Conap) FR-1210 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | IEC 216 |
Dr. D. Mueller Flexiso® DMD FI 14010 00360 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00360 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Trelleborg Emerson & Cuming Stycast® XT-1169 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Von Roll Isola IMI Varnish 3405 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: |