Material Notes:
Neoplast 145 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 47
47
ASTM D 2240
49

@Time 605000 sec
49

@Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 3.14 MPa
455 psi
500 mm/min; ASTM D 412
2.55 MPa

@Time 605000 sec
370 psi

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 325 %
325 %
500 mm/min; ASTM D 412
244 %

@Time 605000 sec
244 %

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.00108 GPa
0.156 ksi
500 mm/min; ASTM D 412
Tear Strength 10.8 kN/m
61.6 pli
500 mm/min; ASTM D 624
Compression Set 15 %

@Temperature 23.0 °C,
Time 79200 sec
15 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Brittleness Temperature -62.0 °C
-79.6 °F
ASTM D 746