Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.55 MPa | 370 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Tensile Strength, Ultimate | 2.55 MPa | 370 psi | |
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Tensile Strength, Ultimate | 2.55 MPa | 370 psi | |
Momentive Performance Materials RTV106 Red Adhesive Sealant, High Strength, High Temperature Paste One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance.. |
|||
Tensile Strength, Ultimate | 2.55 MPa | 370 psi | JIS K6301 |
Stellarchem GP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Tensile Strength, Ultimate | 2.55 MPa @Time 605000 sec |
370 psi @Time 168 hour |
Heat Aging; ASTM D 412/ASTM D 573 |
Zylog Neoplast® 145 FT EB Thermoplastic Vulcanizate Neoplast 145 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, .. |