Material Notes:
Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This material also has a high heat deflection temperature, good creep resistance, tensile and flexural strength and high rigidity. It has outstanding electrical properties, even at high frequencies and temperatures and is rated UL94 V-0 at 1/32" or 0.031"(0.8 mm) in all colors. Humidity resistance is another key feature. Mindel B-322 retains a high level of mechanical and electrical properties even at elevated temperatures, which can make it a suitable replacement for high performance thermosets. - Black: Mindel B-322 BK 1045
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Water Absorption 0.14 %

@Time 86400 sec
0.14 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 4.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 275 °C
4.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength 103 MPa
14900 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 159 MPa
23100 psi
ASTM D790
Flexural Modulus 6.89 GPa
999 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Tensile Impact Strength 84.1 kJ/m²
40.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
15.0 µin/in-°F
ASTM D696
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed; ASTM D648
UL RTI, Electrical 160 °C
320 °F
UL 746
UL RTI, Mechanical with Impact 160 °C
320 °F
UL 746
UL RTI, Mechanical without Impact 160 °C
320 °F
UL 746
Flammability, UL94 V-0

@Thickness 0.790 mm
V-0

@Thickness 0.0311 in
UL 94
Oxygen Index 35 %
35 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
ASTM D150
3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
ASTM D150
3.7

@Frequency 60.0 Hz
3.7

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm

@Thickness 1.60 mm
508 kV/in

@Thickness 0.0630 in
Method B (Step-by-Step); ASTM D149
20.0 kV/mm

@Thickness 3.18 mm
508 kV/in

@Thickness 0.125 in
Method A (Short-Time); ASTM D149
29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
Method B (Step-by-Step); ASTM D149
30.0 kV/mm

@Thickness 0.800 mm
762 kV/in

@Thickness 0.0315 in
Method A (Short-Time); ASTM D149
Dissipation Factor 0.0020

@Frequency 60.0 Hz
0.0020

@Frequency 60.0 Hz
ASTM D150
0.0030

@Frequency 1000 Hz
0.0030

@Frequency 1000 Hz
ASTM D150
0.0090

@Frequency 1.00e+6 Hz
0.0090

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 125 sec
125 sec
ASTM D495
Processing Properties Metric English Comments
Melt Temperature 271 - 316 °C
520 - 601 °F
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Drying Temperature 135 - 163 °C

@Time 10800 - 14400 sec
275 - 325 °F

@Time 3.00 - 4.00 hour
Moisture Content 0.020 %
0.020 %
Descriptive Properties Value Comments
Additive Flame Retardant
Appearance Colors Available
Natural Color
Availability Asia Pacific
Europe
North America
South America
Features Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
High Rigidity
Warp Resistant
Forms Pellets
Processing Method Injection Molding
RoHS Compliance RoHS Compliant
Suggested Max Regrind, % 25
Uses Appliance Components
Appliances
Business Equipment
Electrical Housing
Electrical Parts
Electrical/Electronic Applications
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved