| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183-A |
|
Okulen® 2000 PE-UHMW, F-Ex
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | TA4310B |
|
Permabond TA4310 Toughened Acrylic Adhesive
PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | Finaprene 2602 |
|
Total Finaclear® 520 Clear Impact Polystyrene
(discontinued **)
Finaclear® 520 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles. Complemented by inherent repr..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | |
|
Premix Thermoplastics PRE-ELEC® PE 1313
(discontinued **)
PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: BK12 is an SBC consisting of KR01 grade with a mold release added for easier processing. BK12 molded parts give excellent detail on fast production cyc..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on f..
|
|||
| Density | 1.01 - 1.07 g/cc | 0.0365 - 0.0387 lb/in³ | ASTM D 792 |
|
Karina E 4048/1-TRE Kariprene Black
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PP CO GF15 CC 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc.
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP
LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized.
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer
Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin..
|
|||
| Density |
1.01
g/cc @Temperature 240 °C |
0.0365
lb/in³ @Temperature 464 °F |
Melt |
|
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j..
|
|||
| Density |
1.01
g/cc @Temperature 240 °C |
0.0365
lb/in³ @Temperature 464 °F |
Melt |
|
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® ELX 50 HNZ TPA
Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® L 20 nat PA12
Medium viscosity unmodified Polyamide 12Information provided by EMS Grivory
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | |
|
Cytec EN-9 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® XE 3817 black 9992 PA12
Product description: Grilamid XE 3817 black 9992 is a medium viscosity, heat and UV-stabilized Polyamid 12. Grilamid XE 3817 black 9992 is especially suitable for the coating of metal tubes and offe..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® L 20H FWA nat PA12
Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | |
|
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
|
Arkema Group Pebax® 4033 Polyether Block Amide (PEBA)
Typical application: Mechanical partsInformation provided by Arkema Group
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | |
|
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
|
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Dry)
Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent...
|
|||
| Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183/A |
|
Addiplast Addilene H 210 G20 Polypropylene Homopolymer
Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast.
|
|||
| Density | 1.01 - 1.08 g/cc | 0.0365 - 0.0390 lb/in³ | |
|
3M 32665 Green Heavy Duty Performance Coating - Part B