Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.07 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
SABIC Innovative Plastics Cycolac® INP581 ABS
High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for..
Density 1.07 g/cc
0.0387 lb/in³
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792, ISO 1183
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
Density 1.07 - 1.26 g/cc
0.0387 - 0.0455 lb/in³
Average value: 1.12 g/cc Grade Count:17
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Density 1.07 g/cc
0.0387 lb/in³
Ineos ABS Lustran® SAN 51
Key Features:UnfilledSuitable processing methods:Injection molding
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
IRPC Polimaxx Polene 2511HX GA5 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 25% GLASS FIBRE REINFORCED VERY HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, LOW SHRINKAGE, HIGH STIFFNESS, CONTAIN UV STABILIZER AND LONG TERM..
Density 1.07 g/cc
0.0387 lb/in³
ASTM D1505
M. Holland Company SA400 Styrene Acrylonitrile
High clarityGood processabilityHigh stiffnessApplications: AppliancesCosmeticsHousehold goods
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade
Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles.
Density 1.07 g/cc
0.0387 lb/in³
LATI Latamid SP1 PA 6.10
Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..
Density 1.07 g/cc
0.0387 lb/in³
Struktol VP 3643 Optimized elastomer-modified epoxy prepolymer
Optimized elastomer-modified epoxy prepolymer for the flexibilisation of epoxy resin systemsApplications: STRUKTOL VP 3643 is used when conventional epoxy systems do not meet the requirements regard..
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Styrolution Luran® S KR 2859 ASA
Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Techmer ES Statiblend® HIPS E AS
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and High Impact ResistanceAppearance: Natural ColorInformation provided by TP Composites, Inc.
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Styrolution Terblend® N NM-11 ABS/PA6 (Dry)
Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which..
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Styrolution Terblend® N NM-13 ABS+PA (Conditioned)
Description: Terblend® N NM-13 is ABS/PA blend combining excellent impact strength at low temperatures with easy processability and good surface appearance.Information provided by STYROLUTION, wh..
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Styrolution Terblend® S NM-31 ASA / PA
Terblend® S is a UV-stabilized ASA/PA blend with high impact strength, easy flow and pronounced color fastness. It is especially suitable for unpainted highly UV-exposed automotive interior parts..
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Tipco Tipcolene® FPC 20 - 20% Calcium Carbonate Reinforced Polypropylene Homopolymer
20% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow
20% Mineral Reinforced, PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Density 1.07 g/cc
0.0387 lb/in³
GB/1033
Zhejiang Juner JEPPB003 High Glossy PP
Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd.
Density 1.07 g/cc
0.0387 lb/in³
(DAM); ISO 1183
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.07 g/cc
0.0387 lb/in³
ASTM Data
Dow Tyril® 125 SAN
Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov..
Density 1.07 g/cc
0.0387 lb/in³
Base
3M Scotch-Weld™ DP8405NS Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP8405NS is a high performance, two-part acrylic adhesives that offer excellent shear, peel and impact performance. These toughened adhesives provide improved adh..
Density >= 1.07 g/cc
>= 0.0387 lb/in³
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Density 1.07 g/cc
0.0387 lb/in³
A. Schulman ComAlloy Comtuf® 602 Nylon 6/6, High Impact Modified
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Density 1.07 g/cc
0.0387 lb/in³
A. Schulman ComAlloy Comtuf® 607 Nylon 6/6, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® M104 MPPO Resin
Flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
PlastxWorld CEVIAN®-V T150 ABS
Medium impact transparent ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.