Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 30 µm | <= 30 µm | 90% smaller than |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 30 - 50 µm | 30 - 50 µm | Mean |
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 30 - 40 µm | 30 - 40 µm | Average; for outer type spray system; Microtrac HRA |
NYC YT3WBHQ Y2O3 Powder for Spray Coating High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c.. |
|||
Particle Size | 30 µm | 30 µm | Geon® DFT 1466; Internal Method |
PolyOne Geon™ FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 50 is a low molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduce.. |
|||
Particle Size | 30 µm | 30 µm | Geon® DFT 1466; Internal Method |
PolyOne Geon™ FIT E 51 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 51 is a medium molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and red.. |
|||
Particle Size | 30 µm | 30 µm | Mean Volume, Geon® DFT 1466; Internal Method |
PolyOne Geon™ FIT E 52 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 52 is a high molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduc.. |
|||
Particle Size | 30 - 70 µm | 30 - 70 µm | d50 |
Magyar Aluminum ALO-P54 Alumina Alumina for Polishing |
|||
Particle Size | <= 30 µm | <= 30 µm | 99% finer |
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 30 µm | 30 µm | 75% finer than |
Imerys Minsilsparâ„¢ Feldspar Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys |
|||
Particle Size | >= 30 µm | >= 30 µm | 0.3% finer than |
Imerys Minsparâ„¢ 1 Feldspar Minspar 1 is a minus 30 mesh Feldspar product used in the glass container and ceramic tile markets.Information provided by Imerys |
|||
Particle Size | 30 - 46 µm | 30 - 46 µm | |
Lucite International Colacryl ® B866 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based homopolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.. |
|||
Particle Size | 30 - 37 µm | 30 - 37 µm | |
H.C. Starck Amperit® 146.3 Chromium (Cr) HS Number: 81122031 |
|||
Particle Size | 30 - 38 µm | 30 - 38 µm | 50% |
H.C. Starck Amperit® 558.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 30 µm | 30 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 707 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | <= 30 µm | <= 30 µm | Average size before sieving |
Shanghai Ofluorine 9202F PVDF Powder for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |
|||
Particle Size | 30 µm | 30 µm | |
Silberline Sparkle Silver® 3141-ST Sparkle Silver® 3141-ST is a coarse high sparkle, non-leafing aluminum pigment popular for Automotive Applications. This pigment can be used with tints to produce a wide range of polychromatic ef.. |
|||
Particle Size | 30 µm | 30 µm | |
Silberline Sparkle Silver® 3166-AR Sparkle Silver® 3166-AR is a coarse high sparkle, non-leafing aluminum pigment popular for Automotive Applications. This pigment can be used with tints to produce a wide range of polychromatic ef.. |
|||
Particle Size | 30 µm | 30 µm | |
Shin-Etsu Silicones KSP-102 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 30 µm | 30 µm | 98% less than value (Size C) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 30 µm | 30 µm | 99.5% less than value (Size D) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | <= 30 µm | <= 30 µm | |
Epoxy Technology EPO-TEK® B912-8 Epoxy Product Description: A single component, thermally and electrically conductive, epoxy adhesive designed for semiconductor die attach and circuit assembly applications. Its unique features are a pot.. |
|||
Particle Size | <= 30 µm | <= 30 µm | |
Epoxy Technology EPO-TEK® OG159-2 UV Cure Optical Epoxy Material Description: A single component, high viscosity, UV curable epoxy adhesive designed for sealing glass plates together in the LCD/OLED/display industry. It contains 1mil glass beads for bon.. |
|||
Particle Size | 30 µm | 30 µm | 10th% |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 30 µm | 30 µm | 10th% |
3M K1 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 30 µm | 30 µm | |
3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tan.. |
|||
Particle Size | 30 µm | 30 µm | |
3M Dyneon™ PFA 6503PBZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications i.. |
|||
Particle Size | 30 µm | 30 µm | 50th% |
3M S60 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 30 - 100 µm | 30 - 100 µm | D10-D90 |
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe.. |
|||
Particle Size | 30 - 50 µm | 30 - 50 µm | mean value |
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 30 - 38 µm | 30 - 38 µm | 50% |
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |